1.pider Web or Detachment
Due to improper tension of the quill, excessive lateral movement of the tube and spindle shafts, poor operation, damage to the grooves at both ends of the quill, and other reasons, the yarn at both ends of the quill, especially at the large end of the quill, intermittently or continuously slips off. In severe cases, this forms a spider web quill. This type of defect will cause serious breaks in the yarn during unwinding.
2.Overlapping Knot
Due to failure of the anti-overlapping function, damage to the grooves of the quill, rough obstruction in the yarn channel, and other reasons, the yarn on the surface of the quill overlaps and forms knots, creating an overlapping quill. The overlapping yarn is subject to excessive wear, prone to breakage, and difficult to unwind.
3.Irregular shape
When the intersection of the grooves on the quill is rough, when the clearing plate is blocked by flowery clothes, and when the tension device is misaligned, the yarn guide movement becomes smaller, resulting in gourd-shaped cones; improper operation and misalignment of the cone position lead to capped cones; a fault in the broken end stop mechanism results in raised ring cones; excessive winding tension or incorrect positioning of the spindle tube leads to bell-shaped cones; on a winding machine driven by the spindle shaft, wear at the turning point of the forming cam or displacement between the forming cam and the spindle can cause protrusions or indentations at both ends of the cone.
4.Loose-fitting tube and tight-fitting tube
Improper process settings of the tension device or inappropriate pressure compensation in the cone holder can result in excessively high or low tension, leading to tight or loose cones respectively; foreign objects like flyaway fibers embedded in the tension disc or extremely low relative humidity in the workshop can cause loose cones with very low winding density, which have poor stability and may cause loops to fall off during unwinding.
5.Mismatched Bobbin Sizes
Incorrect judgment by operators often results in mismatched bobbin sizes, affecting the production efficiency of subsequent processes and leading to an increase in the amount of yarn at the base of the bobbin. The use of a fixed-length winding device for the bobbin can overcome this flaw.
The reasons for the generation of intrinsic defects in bobbin yarns.
1. Poor Splicing
The splicing tool is not functioning properly; when the spool breaks, the operation of the joint is not standardized, causing the shape of the joint and the length of the yarn tail to not meet the standards, such as uneven joints, loose joints, looped joints, etc. These poor joints will come apart again in the subsequent production process, leading to broken ends.
2. Incorporation of Fly and Waste Yarn
The electronic yarn clearer is malfunctioning; the yarn catcher is blocked, or the suction nozzle brings in waste yarn; when there is fly or waste yarn on the yarn path or if the operation is not careful, it can cause the fly and waste yarn to be wound into the spool along with the yarn.
3.Excessive Splices
The sensitivity of the electronic clearer is set too high or the splice adjustment is improper.
4.Raw Material Mix-up
Incorrect Batch: Due to poor production management, yarns with different linear densities, batch numbers, and even different colors are mixed and wound on the same bobbin or batch. In subsequent processing steps, such defective bobbins are difficult to detect, and ultimately "incorrect warp" and "incorrect weft" defects appear on the surface of the finished product.
5.Yarn Abrasion
The failure of the automatic stop device for broken ends, not shutting down the machine at the time of breakage, or the presence of burrs on the surface of the quill (drum) can all lead to excessive wear of the yarn, increased fuzz on the yarn body, and a reduction in the strength of the single yarn.
Intrinsic defects in the quill also include double yarns, oil stains, and overlapping ends, among others.
The high degree of automation of the automatic winding machine greatly eliminates the dependence on human factors for high-quality and high-yield winding. The quality assurance system formed by perfected winding technology and strengthened production management ensures that the above-mentioned external and internal defects of the quill are avoided.